2022-01-10
767
![]() |
奧氏體不銹鋼 | UNS牌號:S31703 | 通用材料牌號:317L | |||||||||||||||||
序號 | 類別 | 材料牌號 | 引用標準 | 化學成分 | 機械性能 | |||||||||||||||
C | Mn | P | S | Si | Ni | Cr | Mo | N | 其它 |
屈服 強度σ0.2 |
拉伸 強度 |
延伸率 (縱向) |
硬度 |
斷面 收縮率 |
熱處理 | |||||
% | % | % | % | % | % | % | % | % | % | % | (MPa) | (MPa) | % | HBW | (%) | ℃/冷卻 | ||||
1 | 美標管件 | WP317L | ASTM A403/403M-20 | ≤0.030 | ≤2.00 | ≤0.045 | ≤0.030 | ≤1.00 | 11.0-15.0 | 18.0-20.0 | 3.0-4.0 | ≥205 | ≥515 | ≥28 | ≥1040℃/水冷 | |||||
2 | 美標鋼管 | TP317L | ASTM A312/312M-21 | ≤0.035 | ≤2.00 | ≤0.045 | ≤0.030 | ≤1.00 | 11.0-15.0 | 18.0-20.0 | 3.0-4.0 | ≥205 | ≥515 | ≥35 | 1040℃/水冷 | |||||
3 | 美標板材 | 317L | ASTM A240/A240M-20 | ≤0.030 | ≤2.00 | ≤0.045 | ≤0.030 | ≤0.75 | 11.0-15.0 | 18.0-20.0 | 3.0-4.0 | ≤0.10 | ≥205 | ≥515 | ≥40 | ≤217 | ||||
4 | 美標鍛件 | F317L | ASTM A182/182M-21 | ≤0.030 | ≤2.00 | ≤0.045 | ≤0.030 | ≤1.00 | 11.0-15.0 | 18.0-20.0 | 3.0-4.0 | ≥170 | ≥485 | ≥30 | ≥50 | 1040℃/水冷 | ||||
5 | 國標管件 | |||||||||||||||||||
6 | 國標鋼管 |
022Cr19Ni13Mo3 (S31703) |
GB/T14976-2012 | ≤0.030 | ≤2.00 | ≤0.035 | ≤0.030 | ≤1.00 | 11.00-15.00 | 18.00-20.00 | 3.00-4.00 | ≥175 | ≥480 | ≥35 | 1010-1150℃ /水冷 | |||||
7 | 國標鍛件 |
022Cr19Ni13Mo3 (S31703) |
NB/T47010-2017 | ≤0.030 | ≤2.00 | ≤0.035 | ≤0.015 | ≤1.00 | 11.00-15.00 | 18.00-20.00 | 3.00-4.00 | ≥195 |
≥480 ≥460 |
≥35 |
128-187 121-187 |
1010-1150℃ /水冷 | ||||
8 | 歐標管件 | 1.4438 | EN10253-4:2008 | ≤0.030 | ≤2.00 | ≤0.040 | ≤0.015 | ≤1.00 | 13.00-16.00 | 17.50-19.50 | 3.00-4.00 | ≤0.11 |
σ0.2≥220 σ1.0≥250 |
490-690 | ≥35 | ≤200 |
at-196℃ ≥60 |
1100-1160℃ /水冷 | ||
9 | 歐標鍛件 |